ASTM A515 tērauda plāksne ir specifikācija spiedientvertņu plāksnēm, kas paredzētas lietošanai mērenā vai augstā temperatūrā. Šo materiālu galvenokārt izmanto spiedtvertņu un rūpniecisko katlu ražošanā, kur būtiska ir augsta izturība un lieliska izturība. Tajā ietilpst trīs pakāpes: ASTM A515 60. pakāpe, 65. pakāpe un 70. pakāpe.
Standarts: ASTM A515/A515M
Tērauda marka: A515 GR 60 (415), A515 GR 65 (450), A515 GR 70 (485)
Biezums: 3-500 mm
Platums: 1000-4000 mm
Garums: 1000-18000 mm
Ķīmiskā sastāva prasības
| ASTM A515 spiedtvertņu plāksnes | ||||
|---|---|---|---|---|
| Elements | Gr. 60 | Gr. 65 | Gr. 70 | |
| C maks |
t mazāks vai vienāds ar 1" | 0.24 | 0.28 | 0.31 |
| 1"< t ≤2" | 0.27 | 0.31 | 0.33 | |
| 2"< t ≤4" | 0.29 | 0.33 | 0.35 | |
| 4"< t ≤8" | 0.31 | 0.33 | 0.35 | |
| t>8" | 0.31 | 0.33 | 0.35 | |
| Mn maks |
*H.A. | 0.90 | 0.90 | 1.20 |
| *P.A. | 0.98 | 0.98 | 1.30 | |
| P | maks | 0.025 | 0.025 | 0.025 |
| S | maks | 0.025 | 0.025 | 0.025 |
| Si | *H.A. | 0.15–0.40 | 0.15–0.40 | 0.15–0.40 |
| *P.A. | 0.13–0.45 | 0.13–0.45 | 0.13–0.45 | |
Stiepes prasības
| ASTM A515 | *T.S. MPa [ksi] |
*Y.S. MPa [ksi] |
*EL. 8" min. % |
*EL. 2" min. % |
|---|---|---|---|---|
| 60. klase | 415–550 [60–80] |
Lielāks vai vienāds ar 220 [Lielāks vai vienāds ar 32] |
21 | 25 |
| 65. klase | 450–585 [65–85] |
Lielāks vai vienāds ar 240 [Lielāks vai vienāds ar 35] |
19 | 23 |
| 70. klase | 485–620 [70–90] |
Lielāks par vai vienāds ar 260 [Lielāks vai vienāds ar 38] |
17 | 21 |
Lietojumprogrammas

ASTM A515 tērauda plāksnes parasti izmanto:
- Spiedientvertņu ražošana naftas un gāzes rūpniecībai.
- Katlu un siltummaiņu izbūve.
- Rūpniecisko uzglabāšanas tvertņu un citu spiedienu{0}}jutīgu iekārtu izgatavošana.
- Lietojumprogrammas, kur nepieciešama augsta izturība un izturība, jo īpaši augstas{0}}temperatūras vidēs.
- Rezumējot, ASTM A515 tērauda plāksnes nodrošina robustu un uzticamu risinājumu dažādiem lietojumiem spiedtvertņu un katlu ražošanas sektoros, nodrošinot drošību un veiktspēju prasīgos apstākļos.
Ja vēlaties uzzināt vairāk par GNEE produktiem, varat sūtīt e-pastu uzalloy@gneesteelgroup.com.Mēs esam vairāk nekā priecīgi jums palīdzēt.
| Spiedientvertņu plātņu kategorijas, ko nodrošina GNEE | |||||
| ASTM | ASTM A202/A202M | ASTM A202 A klase | ASTM A202 B pakāpe | ||
| ASTM A203/A203M | ASTM A203 A klase | ASTM A203 B pakāpe | ASTM A203 D klase | ASTM A203 E pakāpe | |
| ASTM A203 F pakāpe | |||||
| ASTM A204/A204M | ASTM A204 A klase | ASTM A204 B pakāpe | ASTM A204 C pakāpe | ||
| ASTM A285/A285M | ASTM A285 A klase | ASTM A285 B pakāpe | ASTM A285 C pakāpe | ||
| ASTM A299/A299M | ASTM A299 A klase | ASTM A299 B pakāpe | |||
| ASTM A302/A302M | ASTM A302 A klase | ASTM A302 B pakāpe | ASTM A302 C pakāpe | ASTM A302 D pakāpe | |
| ASTM A387/A387M | ASTM A387 5. klase 1 | ASTM A387 5. pakāpe, 2. klase | ASTM A387 11. klase 1. klase | ASTM A387 11. klase, 2. klase | |
| ASTM A387 12. klase 1. klase | ASTM A387 12. klase 2. klase | ASTM A387 22. klase, 1. klase | ASTM A387 22. klase 2. klase | ||
| ASTM A515/A515M | ASTM A515 60. klase | ASTM A515 65. klase | ASTM A515 70. klase | ||
| ASTM A516/A516M | ASTM A516 55. klase | ASTM A516 60. klase | ASTM A516 65. klase | ASTM A516 70. klase | |
| ASTM A517/A517M | ASTM A517 A klase | ASTM A517 B pakāpe | ASTM A517 E pakāpe | ASTM A517 F klase | |
| ASTM A517 P klase | ASTM A517 J klase | ||||
| ASTM A533/A533M | ASTM A533 A klase 1 | ASTM A533 B klase 1 | ASTM A533 C klase 1 | ASTM A533 D klase 1 | |
| ASTM A533 A klase 2 | ASTM A533 B klase 2 | ASTM A533 C klase 2 | ASTM A533 D klase 2 | ||
| ASTM A533 A klase 3 | ASTM A533 B klase 3 | ASTM A533 C klase 3 | ASTM A533 D klase 3 | ||
| ASTM A537/A537M | ASTM A537 1. klase | ASTM A537 2. klase | ASTM A537 klase 3 | ||
| ASTM A612/A612M | ASTM A612 | ||||
| ASTM A662/A662M | ASTM A662 A klase | ASTM A662 B pakāpe | ASTM A662 C pakāpe | ||
| LV | EN10028-2 | EN10028-2 P235GH | EN10028-2 P265GH | EN10028-2 P295GH | EN10028-2 P355GH |
| LV10028-2 16MO3 | |||||
| EN10028-3 | EN10028-3 P275N | EN10028-3 P275NH | EN10028-3 P275NL1 | EN10028-3 P275NL2 | |
| EN10028-3 P355N | EN10028-3 P355NH | EN10028-3 P355NL1 | EN10028-3 P355NL2 | ||
| EN10028-3 P460N | EN10028-3 P460NH | EN10028-3 P460NL1 | EN10028-3 P460NL2 | ||
| EN10028-5 | EN10028-5 P355M | EN10028-5 P355ML1 | EN10028-5 P355ML2 | EN10028-5 P420M | |
| EN10028-5 P420ML1 | EN10028-5 P420ML2 | EN10028-5 P460M | EN10028-5 P460ML1 | ||
| EN10028-5 P460ML2 | |||||
| EN10028-6 | EN10028-6 P355Q | EN10028-6 P460Q | EN10028-6 P500Q | EN10028-6 P690Q | |
| EN10028-6 P355QH | EN10028-6 P460QH | EN10028-6 P500QH | EN10028-6 P690QH | ||
| EN10028-6 P355QL1 | EN10028-6 P460QL1 | EN10028-6 P500QL1 | EN10028-6 P690QL1 | ||
| EN10028-6 P355QL2 | EN10028-6 P460QL2 | EN10028-6 P500QL2 | EN10028-6 P690QL2 | ||
| JIS | JIS G3115 | JIS G3115 SPV235 | JIS G3115 SPV315 | JIS G3115 SPV355 | JIS G3115 SPV410 |
| JIS G3115 SPV450 | JIS G3115 SPV490 | ||||
| JIS G3103 | JIS G3103 SB410 | JIS G3103 SB450 | JIS G3103 SB480 | JIS G3103 SB450M | |
| JIS G3103 SB480M | |||||
| GB | GB713 | GB713 Q245R | GB713 Q345R | GB713 Q370R | GB713 12Cr1MoVR |
| GB713 12Cr2Mo1R | GB713 13MnNiMoR | GB713 14Cr1MoR | GB713 15CrMoR | ||
| GB713 18MnMoNbR | |||||
| GB3531 | GB3531 09MnNiDR | GB3531 15MnNiDR | GB3531 16MnDR | ||
| DIN | DIN 17155 | DIN 17155 HI | DIN 17155 HII | DIN 17155 10CrMo910 | DIN 17155 13CrMo44 |
| DIN 17155 15Mo3 | DIN 17155 17Mn4 | DIN 17155 19Mn6 | |||