A516 spiediena tvertnes oglekļa tērauda plāksne
SA516 ir oglekļa tērauda loksnes, ko galvenokārt izmanto metinātām spiediena tvertnēm vidējā un zemā temperatūrā. Materiāls ir pieejams 55., 60., 65. un 70. klasē. Materiāls ir pieejams arī normalizētā stāvoklī, kad nepieciešama uzlabota roba izturība.
A516 Viegla tērauda spiedtvertnes ķīmiskais sastāvs
| Ķīmiskais sastāvs | Maksimālais C % biezumam t (mm) | Mn % priekš biezums t (mm) |
Si % | P % maks |
S % maks |
||||
|---|---|---|---|---|---|---|---|---|---|
| 6-12,5 mm | 12,5-25 mm | 25-50 mm | >50 mm | Mazāks vai vienāds ar 12,5 mm | >12,5 mm | ||||
| A516 Gr55 | 0.18 | 0.20 | 0.22 | 0.25 | 0.55-0.98 | 0.60-1.30 | 0.13-0.45 | 0.035 | 0.035 |
| A516 Gr60 | 0.21 | 0.23 | 0.23 | 0.25 | 0.6-0.9 | 0.80-1.20 | 0.13-0.45 | 0.035 | 0.035 |
| A516 Gr65 | 0.24 | 0.26 | 0.26 | 0.28 | 0.85-1.20 | 0.85-1.20 | 0.13-0.45 | 0.035 | 0.035 |
| A516 Gr70 | 0.27 | 0.28 | 0.28 | 0.30 | 0.85-1.20 | 0.85-1.20 | 0.13-0.45 | 0.035 | 0.035 |
A516 oglekļa tērauda spiedtvertnes mehāniskās īpašības
| Mehāniskais īpašums | Stiepes spēks (MPa) |
Minimums raža spēks (MPa) |
Minimālais pagarinājuma (%) mērierīces garums | |
|---|---|---|---|---|
| 50 mm | 200 mm | |||
| A516 Gr55 | 380-515 | 205 | 27 | 23 |
| A516 G 60 | 415 - 550 | 220 | 25 | 21 |
| A516 Gr65 | 450 - 585 | 240 | 23 | 19 |
| A516 Gr70 | 485 - 620 | 260 | 21 | 17 |
A516 spiedtvertņu tērauda apvalka plākšņu krājumu izmēri
| GRAD | GAUGE (collas) | PLATUMS (collas) | GARUMS (collas) |
|---|---|---|---|
| A516/SA516 | 0.1875 | 96 | 240/480 |
| A516/SA516 | 0.2500 | 96/120 | 240/480 |
| A516/SA516 | 0.3125 | 96/120 | 240/480 |
| A516/SA516 | 0.3750 | 96/120 | 240/480 |
| A516/SA516 | 0.5000 | 96/120 | 240/480 |
| A516/SA516 | 0.6250 | 96/120 | 240/480 |
| A516/SA516 | 0.7500 | 96/120 | 240/480 |
| A516/SA516 | 0.8750 | 96/120 | 240/480 |
| A516/SA516 | 1.0000 | 96/120 | 240/480 |
| A516/SA516 | 1.1250 | 96/120 | 240/480 |
| A516/SA516 | 1.2500 | 96/120 | 240/480 |
| A516/SA516 | 1.5000 | 96/120 | 240/480 |
| A516/SA516 | 1.7500 | 96/120 | 240/480 |
| A516/SA516 | 2.0000 | 96/120 | 240/480 |
| A516/SA516 | 2.2500 | 96/120 | 240/480 |
| A516/SA516 | 2.5000 | 96/120 | 240/480 |
| A516/SA516 | 2.7500 | 96/120 | 240/480 |
| A516/SA516 | 3.0000 | 96/120 | 240/480 |
| A516/SA516 | 3.2500 | 96/120 | 240 |
| A516/SA516 | 3.5000 | 96/120 | 240 |
| A516/SA516 | 3.7500 | 96/120 | 240 |
| A516/SA516 | 4.0000 | 96/120 | 240 |
| A516/SA516 | 5.0000 | 96 | 240 |
| A516/SA516 | 6.0000 | 96 | 240 |
Karsti velmētas katlu tērauda plāksnes Produkta attēls



GNEE grupas komandas foto

GNEE grupas klientu apmeklējums






GNEE Group tērauda izstāde






Mums ir pietiekami daudz krājumu, un mēs varam iepakot un nosūtīt visīsākajā laikā. Ja jums ir vajadzīgas A516 spiedtvertņu oglekļa tērauda plāksnes vai citi karsti velmēti tērauda izstrādājumi, lūdzu, sazinieties ar mani.
Populāri tagi: A516 spiedtvertņu oglekļa tērauda plāksne, Ķīna A516 spiedtvertņu oglekļa tērauda plākšņu ražotāji, piegādātāji, rūpnīca